Say when dimensions apply
Anodize grows about half into and half out of the surface; plating adds thickness on every face. State whether a dimension applies before or after the finish, especially on fits and threads.
Capabilities · Finishing through vetted partners
Every finish on this page is a special process at vetted (incl. Nadcap) partners — none of them is done in-house. We machine the part, allow for coating growth where the finish adds thickness, and coordinate the finish with your vendors or ours. Below is how to call each finish out on the drawing.
Need this part made with a finish? Get a quote01 · Who does what
Machining, wire EDM, grinding, deburr and inspection run on our own floor in Buellton. Finishing and heat treatment are special processes at vetted (incl. Nadcap) partners: we coordinate them with your vendors or ours, and flow special-process requirements down under our vendor quality codes (Q1–Q23).
02 · How to call it out
A finish callout names the specification, the type and class, the thickness where the spec allows a range, and anything the processor would otherwise choose for you. Examples follow common drawing practice; confirm the current revision of each specification for your program. Thickness ranges are typical published values. Every process in this table is performed by a vetted partner.
| Finish | Specification | Callout example | Also state | Thickness | By |
|---|---|---|---|---|---|
| Type II anodize (sulfuric) | MIL-PRF-8625 Type II (formerly MIL-A-8625) | ANODIZE PER MIL-PRF-8625, TYPE II, CLASS 2, BLACK. | Class 1 (undyed) or Class 2 (dyed) and the color; sealed by default; masking. | 0.00007–0.001″ total (~½ builds up) | Partner |
| Type III hardcoat | MIL-PRF-8625 Type III | HARD ANODIZE PER MIL-PRF-8625, TYPE III, CLASS 1, 0.0020 ±0.0004 THK. DIMENSIONS APPLY AFTER ANODIZE. | Thickness; whether dimensions apply before or after; unsealed unless you say otherwise. | 0.0005–0.0045″ total, 0.002″ nominal (~½ builds up) | Partner |
| Chem film, hexavalent | MIL-DTL-5541 Type I | CHEM FILM PER MIL-DTL-5541, TYPE I, CLASS 1A. | Class 1A for maximum corrosion protection; Class 3 for low electrical resistance. | 0.00001–0.0001″ | Partner |
| Chem film, trivalent (RoHS) | MIL-DTL-5541 Type II | CHEM FILM PER MIL-DTL-5541, TYPE II, CLASS 3. | Class 3 for grounding and bonding surfaces; Class 1A when corrosion matters more. | 0.00001–0.0001″ | Partner |
| Finish | Specification | Callout example | Also state | Thickness | By |
|---|---|---|---|---|---|
| Passivation (aerospace) | AMS 2700 Method 1 (nitric) / Method 2 (citric) | PASSIVATE PER AMS 2700, METHOD 2 (CITRIC). | The method only if you need to force it; the verification test if the default is not what you want. | No build-up | Partner |
| Passivation (commercial) | ASTM A967 | PASSIVATE PER ASTM A967. | The processor may use any listed nitric or citric method that passes the required test. | No build-up | Partner |
| Electropolish | ASTM B912 | ELECTROPOLISH PER ASTM B912, THEN PASSIVATE PER ASTM A967. | Removal allowance on toleranced features; which surfaces. | Removes ~0.0002–0.0005″ per surface typ. (more when specified) | Partner |
| Finish | Specification | Callout example | Also state | Thickness | By |
|---|---|---|---|---|---|
| Harden and temper | AMS 2759/1 (carbon and low-alloy steel) | 4140 PER AMS 6382. HEAT TREAT PER AMS 2759/1 TO 28–32 HRC. | Material spec, process spec and a hardness window. | — | Partner |
| Age PH stainless | AMS 2759/3 | 17-4PH PER AMS 5643. AGE PER AMS 2759/3 TO H1025. | The aged condition; machining is done in Condition A first. | — | Partner |
| Stress relieve | AMS 2759/11 | STRESS RELIEVE PER AMS 2759/11, 595 °C ± 14 °C, 1 HR. | Temperature and time when the design depends on them. | — | Partner |
| Finish | Specification | Callout example | Also state | Thickness | By |
|---|---|---|---|---|---|
| Electroless nickel | AMS 2404 (ASTM B733 for phosphorus type) | ELECTROLESS NICKEL PER AMS 2404, CLASS 1, 0.0010–0.0015 THK. | Thickness, phosphorus content if it matters, and any post-plate bake. | 0.0003–0.002″ | Partner |
MIL-PRF-8625 superseded MIL-A-8625; legacy MIL-A-8625 callouts are still recognized. AMS 2700 superseded the cancelled QQ-P-35 passivation callout. Gold, tin and nickel plating are also coordinated through partners; send the specification your drawing invokes.
03 · Sequence and dimensions
Anodize grows about half into and half out of the surface; plating adds thickness on every face. State whether a dimension applies before or after the finish, especially on fits and threads.
Threads, precision bores, grounding points and sealing faces are masked when the drawing says so. Put the masking on the drawing, not in an email.
17-4PH is machined in Condition A, aged by the partner, then finish-machined or wire-EDM'd if the tolerance needs it. Passivation comes after the last machining operation.
Cleaning and plating can charge hardened steel with hydrogen. Call out a relief bake (ASTM B850 or AMS 2759/9) after plating parts at about 31 HRC and up.
On a 60° thread, pitch diameter changes by about four times the per-surface thickness. Plan oversize taps or masking on internal threads.
04 · Going deeper
Each finish has a fuller reference page with types, classes, thickness, sealing, passivation methods and heat-treat specifications. Coating build-up by substrate is in the coatings and finishes finder.
Detailed references: Type II vs Type III anodize · citric vs nitric passivation · heat treatment and AMS 2759 · coatings & finishes
Related
6061, 7075 and MIC-6 with anodize and chem film.
17-4PH aging and passivation sequence.
Build-up, specs and properties by substrate.
Thickness, classes, sealing and callouts.
Dissimilar metals and coating choices.
AS9100D, special processes at vetted partners.
Send the drawing description with the finish spec, masking and quantity. We'll plan the sequence and the finishing partner and quote the part complete.