Skip to main content
True Precision Machining

Capabilities · Materials

Stainless steel CNC machining.

17-4PH and other precipitation-hardening grades, plus 303, 304 and 316L — milled, mill-turned and Swiss-turned in Buellton, California. 17-4PH is machined in Condition A and aged to the drawing's H-condition by a heat-treat partner. Passivation is performed by vetted partners to the AMS 2700 or ASTM A967 callout on your print.

Need this part made in stainless? Get a quote

01 · Grades

Stainless grades we machine.

Call out the grade, the specification and the condition. For precipitation-hardening grades, state the aged condition (for example "17-4PH per AMS 5643, H1025"), because the shop machines in Condition A and the condition decides the heat-treat cycle.

Grade Common specs Notes
17-4PH (UNS S17400) AMS 5643 bar · ASTM A564 The precipitation-hardening workhorse. Machined in Condition A, then aged to the H-condition on the drawing.
Custom 455 Per drawing Precipitation-hardening grade; our gallery includes a threaded Custom 455 flange coupling.
303 Per drawing Free-machining austenitic grade for turned parts; its sulfur content makes it a poor choice for welding and harsh corrosion service.
304 / 304L AMS 5513 sheet/plate · AMS 5647 304L bar General-purpose austenitic stainless for manifolds, housings and brackets; work-hardens if the tool rubs.
316L AMS 5653 bar · ASTM A276 / A479 Molybdenum-bearing, low-carbon grade for fluid, medical and pharmaceutical parts and welded assemblies.
440C Per drawing Martensitic grade, hardened by a heat-treat partner when the drawing calls for it.

Material comes from approved aerospace metals distributors with certified mill test reports (CMTR / EN 10204 3.1) traceable to heat lot, DFARS 252.225-7009 compliant.

02 · 17-4PH machining

Machine in Condition A. Age by partner. Finish if the tolerance needs it.

17-4PH ships solution-annealed (Condition A, about 33 HRC) and in that condition machines like 304 stainless. Aging afterwards raises strength and hardness and contracts the part slightly — about 0.0004–0.0006″ per inch at H900 and roughly twice that at H1150. Thin parts get 0.005–0.010″ of finish stock for a post-aging cleanup; thicker parts usually stay inside tolerance without one.

  1. 01

    Machine in Condition A

    Bar arrives solution-annealed. Rough and semi-finish while the material is at its softest.

  2. 02

    Partner aging

    A heat-treat partner ages the parts to the H-condition and specification on the drawing, for example AMS 2759/3.

  3. 03

    Finish if needed

    Aging contracts the part slightly. Tight features are finish-machined or wire-EDM'd after aging; thicker parts often need no finish operation.

  4. 04

    Partner passivation

    Passivation to the AMS 2700 or ASTM A967 callout on the drawing, by a vetted partner.

Common aged conditions (ASTM A564 / AMS 5643 bar minimums)

Condition Aging (air cool) UTS min 0.2% YS min Hardness min
H900 900 °F (482 °C), 1 h 190 ksi 170 ksi 40 HRC
H1025 1025 °F (552 °C), 4 h 155 ksi 145 ksi 35 HRC
H1075 1075 °F (579 °C), 4 h 145 ksi 125 ksi 32 HRC
H1150 1150 °F (621 °C), 4 h 135 ksi 105 ksi 28 HRC

Trade-offs between conditions — toughness and stress-corrosion behavior — are in 17-4PH H900 vs H1025 vs H1075 vs H1150; speeds and feeds by condition are in how to machine 17-4PH.

03 · 300-series

Keep the tool cutting.

Austenitic stainless work-hardens when a tool rubs instead of cuts. The cure is sharp, positive-rake carbide, a feed heavy enough to stay under the hardened layer, no dwell in the cut, and plenty of coolant.

  • 303 vs 304. 303 machines faster and suits turned parts, but its sulfur inclusions lower corrosion resistance and weldability. Specify 304 or 316 if the part is welded or sees chlorides.
  • 316L for fluid and medical work. Low carbon avoids sensitization at welds; electropolish per ASTM B912, when specified, is a partner process.
  • Deep pockets. Deep pockets in 316L run well on the Mori Seiki SH503 horizontal machining center, where chips fall away from the cut instead of being recut.
  • Keep iron out. Tools, wheels and brushes that touch stainless should not touch carbon steel, so free iron is not embedded before passivation.
Turn-milled 17-4PH stainless bore housing
17-4PH bore housing — turning + 5-axis milling
Stainless fitting with a triple-start Acme thread, polished, passivated thread roots
Triple-start Acme, 303/316L — passivated per AMS 2700 by partner
5-axis machined 304 stainless hydraulic manifold
304 stainless hydraulic manifold — 5-axis

04 · Passivation and heat treat

Partner-performed, shop-coordinated.

Passivation and heat treatment are not done in-house: they are special processes at vetted (incl. Nadcap) partners. We coordinate them with your vendors or ours, and flow special-process requirements down under our vendor quality codes (Q1–Q23).

PASSIVATE PER AMS 2700, METHOD 2
Aerospace callout that forces citric. Method 1 is nitric. Citric is the low-risk choice for 17-4PH H900.
PASSIVATE PER ASTM A967
Commercial callout; the processor may use any listed nitric or citric method that passes the required verification test.
AGE PER AMS 2759/3 TO H1025
Precipitation-hardening stainless heat treatment; state the condition and, if it matters, the hardness check.
Free-machining grades
Sulfur-bearing grades such as 303 need citric or a dichromate-inhibited nitric bath; plain nitric can attack the sulfide inclusions.

More: citric vs nitric passivation · heat treatment reference · finishing callout guide

05 · Equipment and inspection

Matched to the part.

Parts are inspected on the 2025 Hexagon Global S CMM and Keyence optical systems before they ship, with AS9102 first articles when your program calls for them and results logged in ProShop against the lot.

  • 5-axis milling

    Doosan DVF 5000 (8 × 500 mm pallets, automated swap) and Kitamura Mytrunnion 4G

  • Mill-turn

    Doosan Puma SMX 2600ST, TT1800SY and Mori Seiki NL2500SY — bar to 3.2" (81 mm)

  • Swiss-type turning

    Tsugami B0205-III (3–20 mm (0.118"–0.787")) and B0326II (32 mm (1.26"))

  • Horizontal milling

    Mori Seiki SH503 — 500 mm pallet, horizontal (gravity chip evacuation)

  • Wire EDM

    Hardened 17-4PH details, slots and sharp inside corners after aging

Stainless part to quote?

Send the grade, condition and passivation callout with the quantity per release. We'll plan the machining, the partner heat treat and passivation, and quote it.